环氧地坪施工前的设计和专业化施工队伍的组织对基层的检查和处理正确的施工组织和质量监督等过程的全程控制。在无锡环氧地坪漆施工前,须清楚了解查看基面状况,下面介绍一般环氧地坪工业环氧地坪漆涂料涂装对地面基层的要求及常见的处理方法。1)水泥基面牢固、结实、不起壳,应杜绝砂浆起壳现象,混凝土层与砂浆找平层最好一起浇筑。若先浇筑混凝土层,则要求砂浆层的厚度不低于40MM,对叉车道的要求则更厚。有关坡度应符合设计要求,允许偏差值的2%,并且不大于30MM。
(2)要求表面不起砂,硬度高,没有水泥粉化现象。新浇筑的水泥砂浆要充分保养。水泥基面平坦,无凹凸不平、蜂窝麻面、水泥疙瘩、其他涂料、乳胶漆、泡泡糖等残渣。(3)表面干燥,含水率小于6%,无油污,PH值应在6.0~8.0;水泥地面养护期过后进场施工前5D,基层不能再用水冲洗或被湿润。
(2) No sand on the surface, high hardness and no cement powdering are required. The newly poured cement mortar should be fully maintained. The cement base surface is flat, without rugged, honeycomb linen, cement bumps, other coatings, latex paint, foam sugar and other residues. (3) The surface is dry, the moisture content is less than 6%, no oil pollution, and the PH value should be 6.0-8.0. After the maintenance period of cement ground, the base can no longer be washed or wetted with water 5 D before construction.
2、基层的检查与预处理基层是环氧树脂地坪涂料的基础,要进行详细检查与分析,以确定其处理措施。
2. The inspection and pretreatment of the base is the basis of epoxy floor coatings. Detailed inspection and analysis are needed to determine the treatment measures.
(1)测量抗压强度。工业环氧地坪的抗压强度不应低于24MPa,为满足某些承重要求,还可能需要更高的强度,应使用回弹仪进行强度测量,或取芯块实测抗压强度。
(1) Measure the compressive strength. The compressive strength of industrial floors should not be less than 24 MPa. In order to meet some important requirements, higher strength may be needed. Strength measurement should be carried out by rebound meter or coring.
(2)确定黏结强度。混凝土基层表面几毫米厚度内通常是水泥浆形成的低强度层。因水泥水化反应导致的收缩,温度变化或荷载的反复作用等产生的应力,会导致黏结强度降低。黏结强度不应低于1.5MPa。
(2) Determine the bond strength. The low strength layer formed by cement slurry is usually in the thickness of several millimeters on the surface of concrete base. The stress caused by shrinkage, temperature change or repeated action of load caused by hydration reaction of cement will lead to the decrease of bond strength. The bond strength should not be less than 1.5 MPa.
(3)基层含水率。只有在水泥基层含水率不大于6%的情况下才能进行涂料的施工,所以含水率的测量尤为重要。确定基层含水率的最佳方法是塑料薄膜覆盖实验法,即将至少1mX1m的聚乙烯薄膜用胶带封粘在混凝土面上,待至少24小时后,根据塑料薄膜上出现冷凝水的数量确定含水率。
(3) Water content of grass-roots. Only when the moisture content of cement base is not more than 6%, can the coating be applied, so the measurement of moisture content is particularly important. The best method to determine the moisture content of the base course is the plastic film covering experiment method, that is, at least 1mX1m polyethylene film is sealed on the concrete surface with tape, and after at least 24 hours, the moisture content is determined according to the amount of condensation water appearing on the plastic film.
(4)环境温度。忽略施工环境温度因素可导致环氧地坪的质量缺陷,例如黏结强度降低、水印、空洞、不规则表面及硬化不兖分等。因此,对于环境温度(气温)、基层表面的温度、露点温度等数所数据,在施工中必须每天测量数次。
(4) Environmental temperature. Ignoring the temperature factors of construction environment can lead to quality defects of epoxy floor, such as reduced bond strength, watermarking, voids, irregular surface and hardening. Therefore, the environmental temperature (air temperature), the surface temperature of the grass-roots, dew point temperature and other data, in the construction must be measured several times a day.
(5)基层清理。对于油脂、机油或有机酸、无机酸或水泥浆所引起的污染,如果不进行彻底清除,将影响环氧地坪漆涂料层的黏结性能。因此地,必须用机械方法清理表面,并通过测定黏结强度进行检查。
(5) grass-roots clean-up. For oil, oil or organic acid, inorganic acid or cement slurry pollution, if not thoroughly removed, will affect the bonding performance of epoxy floor paint coating. Therefore, the surface must be cleaned mechanically and checked by measuring the bond strength.
3、基层处理
3. Grass-roots treatment
(1)为使无锡环氧地坪涂料的施工达到良好的效果,对于尚未找平的地面,应首先施工水泥找平层以进行找平处理。土建方找平时,在水泥初凝时,用专业地面机械对地面进行磨平处理。经过基层处理再涂装的环氧涂装地坪的表面会更平整、光亮,使用寿命也会提高。
(1) In order to achieve good results in the construction of epoxy floor coating, cement leveling layer should be first applied to leveling the ground that has not yet been leveled. When the cement is initially solidified, the civil engineer uses professional ground machinery to grind the ground. The surface of epoxy-coated floor will be smoother, brighter and the service life will be improved after basic treatment and re-coating.
(2)待水泥层干燥后(大约28天),用打磨机对地面进行整体打磨处理,使其表面平整,水泥毛细孔全部敞开。
(2) After the cement layer is dried (about 28 days), the whole ground is polished with a grinder to make the surface smooth and the cement capillary holes open.
(3)对于有油污(食用油、机油)的基层,先用表面处理剂喷洒于用水冲湿的地表面,反复擦洗,直到无油污为止。
(3) For the base layer with oil contamination (edible oil, engine oil), the surface treatment agent is sprayed on the surface wetted with water and scrubbed repeatedly until there is no oil contamination.
盐城雨季高温环氧地坪施工时应注意哪些问题?盐城环氧地坪 连续的橙色高温预警给人们日常生活带来极大不便。尤其是对于盐城环氧地坪的施工人员来说,夏季过高对温度给施工带来很多麻烦,首先要知道温度和湿度对环氧地坪质量的控制。一般情况下施工过程中建议在温度在5℃以上进行施工,认为气温及地面温度过低会严重影响环氧涂料的固化,导致漆膜硬度、强度、光泽度等性能下… 在盐城选择环氧地坪漆需要考虑哪四个因素盐城环氧地坪 任何材料的选择都是需要注重细节因素的,随着盐城环氧地坪漆越来越受欢迎,市场上呈现出了很多的同类品牌。消费者在选择这类产品的时候不仅要注重品牌的选择,更需要注意四个因素。究竟是需要注意哪四个因素呢?接下来就带大家一起来了解一下。环氧地坪漆选择首要考虑的因素就是耐磨性。地坪所能够承受的最大承重力…推荐新闻
聚氨酯地坪漆与环氧地坪漆有什么区别
水性聚氨酯环氧地坪漆和水性环氧地坪漆在使用上大致相同,只是水性聚氨酯无锡环氧地坪漆能在室外使用,而水性环氧地…
环氧地坪的优势及其相关施工位置的要求说明…
环氧地坪是什么呢?想必我们大家都是很熟悉了,不管是在一些地下停车场,还是舞蹈机构的教室中,我们都是可以看到它…
如何处理环氧地坪施工后的起皮和起皮问题?…
一、环氧地坪漆产品质量因素底漆附着力差,环氧树脂材料质量差,会造成地板耐久性、剥离、分层、变色、开裂等,应使…
在盐城环氧地坪施工注意事项及其改造修补方…
在我们的生活中,盐城环氧地坪漆是较为常见的一类涂漆了,不管是在各个企业的车间内,还是各个教育机构的教室内,我…
解析环氧地坪施工中涂附着力差的原因
环氧地坪中涂的作用是增加地坪的厚度,提高地坪的耐磨性能,作为找平层提高地坪的平整性;如果地坪中涂层附着力差,…
在盐城施工高质量的环氧地坪我们需要注意哪…
质量好的盐城环氧地坪一般可以使用5~8年时间,而质量不好的则会在半年之内出现弊病甚至损坏。发生这样问题40%的原因…
建筑施工人员合理选择环氧地坪五点须知
环氧地坪是现代建筑行业用的比较多的一种建筑材料。地坪装饰行业最突出的特点是涂料和涂装的整体结合,涂装和涂层体…
环氧地坪多少一平方?盐城环氧地坪施工报价…
环氧树脂地坪系列包括环氧平面涂层,环氧砂浆地坪,环氧自流平地坪,环氧彩砂地坪,环氧防滑地坪,环氧防静电地坪等…
环氧地坪地坪基层处理不好将会有哪些影响?…
熟话说,根基不稳,在强势的产品终究还会下降的。环氧地坪也是如此,盐城环氧地坪有地坪基层,相当于建房子的地基一…
环氧地坪包工多少钱?怎么施工才性价比高
环氧地坪哪家好?哪里便宜?提起这个问题,我相信大家都是公说公有理,婆说婆有理。要拿出真本事来,才算是好的。其…
管理员
该内容暂无评论